What Is Aluminum Extrusion: A Design Guide to Wall Thickness, Tolerances and Die Types

Mandeep
November 10, 2026

In this note

A customer who was new to aluminum extrusion sent VIA INDIGOS a guard rail section that 2 extruders had already quoted at $6.10 a kilo, and his question was a fair one, because if you ask what is aluminum extrusion priced on, the metal is only about $2.60 of that, so where did the other $3.50 go? Our engineer opened the drawing, found a 4 mm gap on a 30 mm deep channel, and asked whether the gap could be 10 mm without hurting the rail, and it could. That one change turned the section from a semi hollow die into a solid die, the next quote came back at $4.20 a kilo with a die at half the price, and nothing changed on the installed rail. I spent years approving extrusion quotes as a supply chain head without knowing that a 6 mm change on a drawing could do that, because nobody on the extruder side had ever explained it to me. So here is the process from billet to bundle, the 3 die types, and the 12 checks that found that gap.

How the aluminum extrusion process runs, from billet to aged profile

Start with a log of 6063 aluminum, 150 to 250 mm across, cut into billets about a metre long. A billet goes into a furnace and comes out at 450 to 500 °C, soft but solid, and a hydraulic ram on a press of 1,800 to 4,000 tonnes pushes it against a steel die with your section cut through it. The metal flows through the opening at a few metres a minute, is caught on a runout table, and is quenched by air or water as it leaves the die, which locks in the temper.

The profile is then stretched by about 1 to 3 percent between 2 jaws to straighten it, cut to length, and aged in an oven at 180 to 200 °C for several hours, which hardens it to T5 for 6063 or, with a faster quench and sometimes a separate solution treatment, to T6 for 6061, which I covered in the 6061 vs 6063 note. After that comes the aluminum extrusion processing, cutting to final length, punching, CNC machining, anodising or powder coating, and the profile goes into a bundle. Every one of the 12 checks below exists because of something in those 2 paragraphs, and the first 2 checks are about the die itself.

First trial aluminum extrusion section on the tool room bench beside its die at a partner facility in India
First trial section on the bench at one of our manufacturing partners. The 12 checks happen before this moment, and the corrections happen after it

The three die types, and what each one costs you

A solid die is a flat steel disc with the section wire cut through it, and it makes any profile with no enclosed space, angles, channels, flat bars and heat sink fins. It is the cheapest die, the fastest to make, and the most forgiving. A hollow die makes a tube or any profile with an enclosed void, and it does it with a 2 piece tool, a mandrel held on legs that splits the metal into streams which weld back together under pressure behind the mandrel, which is why every hollow extrusion has seam welds you cannot see and why hollow dies cost 2 to 4 times a solid and take 4 to 6 weeks instead of 2 to 4.

A semi hollow die makes a profile with a deep narrow opening that is nearly enclosed, a C channel with a small gap or a screw port, and the die shop treats it as a hollow when the tongue of steel that forms the opening becomes too thin to survive the press load. The rule of thumb is the tongue ratio, the area of the partly enclosed void divided by the square of the gap, and above about 3 the section becomes semi hollow and the die price jumps with it. That is exactly what had happened on the guard rail, and it is the first check for a reason.

The twelve checks our engineers run on every section

This is the sheet our engineer works through with the drawing open, and the plant tool room signs off the same 12 lines before the die is ordered. The values are typical for 6063 and 6061 on mid size presses, and the die shop confirms them for your section, so treat the table as the questions and the quote as the answers.

CheckWhat we look for, typical for 6063 and 6061Why it matters on the pressWhat to write or change
Wall thickness, minimum1.0 mm on small sections, 1.5 to 2 mm over 100 mm acrossthin walls fill late and tear at speedthicken, or accept a slower press and higher $ per kg
Wall thickness, uniformthickest wall no more than 2 to 3 times the thinnestmetal runs fastest through thick walls and twists the profileeven the walls out, or add a web
Circumscribing circleabout 150 mm on a 7 inch press, 250 mm on a 10 inchthe circle picks the press and the press picks the plantstate the circle on the RFQ
Tongue ratiobelow about 3 for a solid dieabove it the tongue breaks, so it becomes semi hollowwiden the gap or shorten the channel
Corner radiiinside 0.5 mm minimum, outside 0.5 to 1 mmsharp corners crack the die and tear the surfaceadd the radius, nobody will see it
Symmetry and balancemass balanced about the centre where function allowsunbalanced sections bow and twist on the runoutadd a balancing fin
Hollow or nothollow only where the function needs a closed voida hollow die costs 2 to 4 times a solidopen the section into a C where you can
Screw ports and snap fitsport sized to the thread, snaps with a lead intight ports strip, stiff snaps crackuse the extruder’s port table
Dimensional toleranceabout ±0.15 mm under 12 mm, ±0.2 to 0.3 mm to 50 mm, wall ±10%what the press holds without a special diewrite the standard, tighten only the few that mate
Straightness, twist, flatnessabout 1 mm per metre, twist about 0.5° per metreset by the stretcher, not the diewrite it only on the length that mates
Finish and exposed faceswhich faces show, anodise or powder, thicknessdie lines show on exposed faces under anodisemark exposed faces so the die is oriented for them
Weight per metre and cut lengtharea in mm² × 2.7 ÷ 1,000 = kg per mweight sets the price, cut length sets the sawput both on the drawing

Twelve lines is a lot to take in from a table, so let me talk you through them in 3 groups, the shape checks, the tolerance checks and the finishing checks.

The shape checks, in plain words

The first 8 lines are about how metal moves through a die, and they come down to one idea, which is that aluminum at 480 °C flows like a very stiff liquid and goes where the opening is widest. A section with a 6 mm wall next to a 1.2 mm wall comes out of the die bent, because the thick side left first, and the plant slows the press and corrects the die to fight it. A sharp inside corner cracks the die tongue after a few thousand kilos, and a channel 30 mm deep with a 4 mm gap has a tongue ratio of about 7, so it is a semi hollow die whether the drawing calls it one or not.

None of these changes alter what the part does, and all of them alter what it costs, which is why the conversion line on the quote is the line design controls, as I showed in the extrusion cost note. On the guard rail, opening the gap from 4 to 10 mm changed nothing the customer could see on the installed rail, and it took $1.90 a kilo off every metre he bought for the next 5 years. The next 2 lines are where buyers over specify, and I did it myself for years.

The tolerance checks, and what counts as standard

The industry standard aluminum extrusion tolerances, published by the Aluminum Extruders Council and the Aluminum Association in the US and in EN 755-9 in Europe, are what a press holds with a normal die and a normal stretch, and they are looser than most drawings written by machinists expect, roughly ±0.15 mm on small dimensions, growing with the dimension, ±10 percent on wall thickness, and straightness of about a millimetre per metre.

Write the standard in the title block and the plant quotes a normal die. Call out 2 or 3 dimensions tighter, a slot that takes a bearing or a face that mates with a machined part, and the plant tells you whether the die can hold it or whether that dimension should be machined after extrusion. Write every dimension tight and you have asked for a die that does not exist, and the quote that comes back will be either very high or quietly ignoring your drawing, and I am not sure which is worse. The last 2 lines are about what happens after the press, and they decide how the part looks on the shelf.

The finishing checks, and who is standing at the press

Anodising builds a coating that is roughly half outward and half into the metal, so a 15 micron anodise adds about 0.008 mm a side, which nobody notices on a frame and everybody notices on a sliding fit. Die lines, the fine marks every extrusion carries along its length, show through a clear anodise and disappear under powder coat, so a section that will be anodised needs its exposed faces marked, and the die shop orients the die so those faces run against the smoothest bearing and away from the mandrel legs on a hollow, and the anodise vs powder coat note covers the choice itself.

Our engineers are in the extrusion plants every day, not on visits, so the die trial, the first bundle and every production run has one of our people at the press with the drawing and these 12 lines in hand, and the weekly tollgate email you get every Friday lists every open item on the die, the date it was promised and the date it will land. I approved extrusion dies for years before anyone explained the tongue ratio to me, and some of those were hollow dies the parts did not need, which is why our manufacturing partners get a section from us only after the 12 checks are done.

Aluminum extrusion profiles racked on an anodising line at a partner facility in India
Racked for anodise at one of our manufacturing partners. The coating grows half out and half in, which is why the sliding fit was dimensioned after anodise

If you have a section that quotes high and you cannot see why, send me the drawing and I will tell you which of the 12 lines is costing you and what to redraw, before you spend a dollar on a die, because a die you did not need is the one cost in extrusion you never get back.

Questions buyers ask us about extrusion design

What is aluminum extrusion?

A process where a heated aluminum billet at 450 to 500 °C is pushed by a hydraulic press through a steel die with the section cut through it, so the profile that comes out has the shape of the opening for any length you want. The profile is quenched, stretched straight, cut and aged to temper, then finished by cutting, machining, anodising or powder coating.

What is the minimum wall thickness for an aluminum extrusion?

About 1.0 mm on small sections and 1.5 to 2 mm on sections over 100 mm across, for 6063 and 6061 on mid size presses. Thinner walls fill late and tear at speed, so the plant slows the press and the price per kilo goes up. Keep the thickest wall within 2 to 3 times the thinnest so the profile comes out straight.

What are standard aluminum extrusion tolerances?

Roughly ±0.15 mm on dimensions under 12 mm, ±0.2 to 0.3 mm up to 50 mm, ±10 percent on wall thickness, straightness about 1 mm per metre and twist about 0.5 degree per metre, per the Aluminum Association and Aluminum Extruders Council standards in the US and EN 755-9 in Europe. Write the standard and tighten only the few dimensions that mate.

Why does a hollow extrusion die cost more?

A hollow die is a 2 piece tool with a mandrel held on legs, so the metal splits around the legs and welds back together behind them, which takes more steel, more machining and more trials. It costs 2 to 4 times a solid die and takes 4 to 6 weeks. A deep narrow channel with a tongue ratio above about 3 is priced as a hollow too, so widening the gap can halve the die price.

Send your drawing.Full landed cost in 5 business days.

DFM notes inside 48 hours. Part price, tooling, freight and duty shown as separate lines. First response inside 24 hours.

Send RFQ now
Mandeep Singh, Co-Founder and CEO of VIA INDIGOS, who writes and reviews the From the floor notes
Reviewed by Mandeep Singh, Co-Founder and CEO, VIA INDIGOS 13+ years buying engineered parts before founding VIA INDIGOS.

This website stores cookies on your computer. Cookie Policy